详细介绍: 不锈钢药芯焊丝
型号
|
抗拉强度σb/Mpa
|
伸长率δ5/%
|
热处理
|
E307TX-X
|
590
|
30
|
-
|
E308TX-X
|
550
|
35
|
E308LTX-X
|
520
|
E308HTX-X
|
550
|
E308MoTX-X
|
E308LMoTX-X
|
520
|
E309TX-X
|
550
|
25
|
E309LNbTX-X
|
520
|
E309LTX-X
|
E309MoTX-X
|
550
|
E309LMoTX-X
|
520
|
E309LNiMoTX-X
|
|
E310TX-X
|
550
|
E312TX-X
|
660
|
22
|
E316TX-X
|
520
|
30
|
E316LTX-X
|
485
|
E317LTX-X
|
520
|
20
|
E347TX-X
|
25
|
E409TX-X
|
450
|
15
|
E410TX-X
|
520
|
20
|
①
|
E410NiMoTX-X
|
760
|
15
|
②
|
E410NiTiTX-X
|
E430TX-X
|
450
|
20
|
③
|
E502TX-X
|
415
|
④
|
E505TX-X
|
E308HMoT0-3
|
550
|
30
|
-
|
E316LKT0-3
|
485
|
E2209T0-X
|
690
|
20
|
E2553T0-X
|
760
|
15
|
EXXXTX-G
|
不规定
|
R308LT1-5
|
520
|
35
|
-
|
R309LT1-5
|
30
|
R316LT1-5
|
485
|
R347T1-5
|
520
|
①加热到730~760℃保温1h后,以不超过55℃h的速度随炉冷至315℃,出炉空冷至室温
|
②加热到595~620℃保温1h后,出炉空冷至室温
|
③加热到760~790℃保温4h后,以不超过55℃h的速度随炉冷至590℃,出炉空冷至室温
|
④加热到840~870℃保温2h后,以不超过55℃h的速度随炉冷至590℃,出炉空冷至室温
|
|